[ Post New Message | Post Reply to this One | Send Private Email to jim megargee | Help ]

Solarization of 665

from jim megargee (mvjim@interport.net)
I dont know if this helps --but-- we often see the "problem" / "effect" when - 1- photographers are working quickly and the negs are being pealed off too soon. (Prior to the necessary 60 sec development / fixing time. 2- The temp. of the materials or the enviroment are below normal. eg. if you are working outside in 50 degree F weather ,665 requires longer development before pealing or warming of the material prior to shooting. One suggestion is that if you are trying to achieve this effect that you give the negative a bit more exposure than normal to achieve an easier printing negative.
(posted 9181 days ago)

[ Previous | Next ]